Moisture-absorbing and sweat-wicking polyester multifunctional finishing agent reaction kettle chemical material technology
Moisture-absorbing and sweat-wicking polyester multifunctional finishing agent reaction kettle chemical material technology
Moisture wicking finishing agent: 100KG
Water: 900KG
1. Pour 900KG of water into the reactor and heat up to 95°C
2. Put 100KG of moisture absorption and perspiration finishing agent into the reactor, keep it at 85°C for 3 hours, keep stirring during the process
3. Keep stirring and wait for natural cooling. (A uniform liquid will be formed at 45°C)
4. unwinding
Moisture wicking finishing agent: 100KG
Water: 900KG
1. Pour 900KG of water into the reactor and heat up to 95°C
2. Put 100KG of moisture absorption and perspiration finishing agent into the reactor, keep it at 85°C for 3 hours, keep stirring during the process
3. Keep stirring and wait for natural cooling. (A uniform liquid will be formed at 45°C)